MCI regional account manager Sean Hightower encourages stakeholders to prepare for the ‘not if, but when’ of concrete cracking.

Does concrete crack just because it is concrete? In some cases, yes, but a deeper issue at stake is corrosion, the primary cause of concrete failure and part of a vicious cycle of concrete deterioration. Whether or not the initial cracks are caused by corrosion or some other force, Migrating Corrosion Inhibitors (MCIs) offer an important strategy to slow down reinforced concrete corrosion and its resulting cracking and spalling at practically any stage of a structure’s life cycle.

The number one cause of concrete failure

Many external forces, such as shrinkage or freeze–thaw cracking, work to eventually fracture the initially unmarred surface of new concrete. However, Sean Hightower, regional account manager for Cortec MCI and former superintendent for custom pool builds, believes that the role of corrosion is underappreciated.

“I’m under the impression that most people think concrete cracks because it is concrete, which isn’t entirely untrue,” he commented. “The old saying rings true more often than not when it comes to concrete cracking, ‘not if but when’; however,” he added, “… the number one cause of concrete failures is actually corrosion of reinforcement steel.”

The vicious cycle of concrete cracking and rebar corrosion

Whatever the cause of that first crack, any fissure in the protective cover opens the path for corrosives such as chloride-rich de-icing salts and ocean spray to enter the concrete and attack the reinforcing metal. Once corrosion of reinforcement steel starts, the rebar begins to swell, putting pressure on the concrete and eventually leading to more cracks, spalling and additional pathways for corrosives to enter and continue the vicious cycle of deterioration. Even structures that were intentionally specified with extra-thick concrete cover for greater durability are vulnerable to corrosion once a crack forms.Not if, but when: using MCI to mitigate corrosion in the presence of concrete cracking

The simplest way to address corrosion at any stage of the concrete life cycle

While many strategies exist to combat corrosion of reinforced concrete, Migrating Corrosion Inhibitors (MCI) stand out as a practical solution because they can be applied at any stage and continue to work in the presence of concrete cracks. MCI delays the onset of corrosion and reduces corrosion rates once it has started by adsorbing onto metal surfaces, forming a protective molecular layer against corrosion reactions.

Concrete construction: The best time to incorporate MCI is during construction. MCI admixtures typically offer cost savings in comparison with other strategies to extend concrete service life, such as epoxy-coated rebar or extra-thick concrete cover.

Concrete maintenance: Existing structures can be fortified by periodic maintenance with an MCI surface-applied corrosion inhibitor (SACI) and/or water repellent.

Concrete repair: MCI SACIs are also important for use during concrete repairs because they can help even out the corrosion potential between patches of new and old concrete, reducing the risk of the ring anode effect. In situations where corrosion is occurring beneath thick concrete cover or under cladding tiles, MCI gel can be injected into the concrete for deeper penetration to reach the embedded rebar.

Planning for the inevitable: corrosion mitigation when concrete cracks

Concrete cracks are inevitable. The important question is how to reduce corrosion even if cracks appear. MCI provides an excellent opportunity to slow down the vicious cycle of deterioration and extend the service life of concrete bridges, car park ramps and other structures.

Contact Cortec for more information about what to do ‘not if, but when’ concrete cracks.